NICKEL ALLOY BALLS
MONEL
Monel is widely used in the chemical, pharmaceutical, maritime, oil, textile and paper industries.
It is highly resistant to (caustic) alcaline solutions, sea water and diluted sulphuric acid.
Monel-K (500) is often used when higher hardness and resistance are needed.
| CHEMICAL COMPOSITIONS
% |
MATERIAL |
Ni |
Al |
Fe |
Mn |
C |
Si |
Cu |
MONEL
400 |
63-70 |
- |
2,50 max |
2,00 max |
0,30 max |
0,50 max |
31,50 max |
MONEL
K 500 |
63-70 |
2-4 |
2 max |
1,50 max |
0,25 max |
1,00 max |
31,50 |
| MATERIAL |
AVERAGE HARDNESS INDEX |
SPECIFIC WEIGHT |
| MONEL 400 |
110/149 BHN |
8,83 |
| MONEL K 500 |
230/315 BHN |
8,46 |
Diameters: from mm 1,50 to mm 150
Precision grades: ISO 3 290 G 100 - G200
HASTELLOY
This material is universally used in valves and pumps where the greatest resistance is required to corrosion caused by strongly oxidising acids.
Hastelloy-C276 is resistant to strongly oxidising agents such as chlorine, nitric, acetic, formic, phosphoric, sulphuric and hydrofluoric acids, zinc chloride and ammonium solutions, water-based solutions containing chlorine or hypochlorites and acid solutions of ferric and cupric salts.
Hastelloy-D is exceptionally resistant to any concentration of sulphuric acid, up to its boiling point.
| CHEMICAL COMPOSITION % |
| MATERIAL |
Cr |
C |
Mo |
Si |
Mn |
Fe |
Ni |
WC |
Co |
| HASTELLOY B2 |
1,00max |
0,02 max |
26,00/30,00 |
0,10 max |
1,00 max |
2,00 max |
65,00/70,00 |
3,00/4.50 |
1,00 max |
| HASTELLOY C276 |
14,50/16,50 |
0,02 max |
15,00/17,00 |
0,8 max |
1,00 max |
4,00/7,00 |
54,00/58,00 |
|
2,50 max |
| HASTELLOY D |
1,00 max |
0,12 max |
|
7.50/10,00 |
0,5/1,25 |
2,00 max |
84,00/86,00 |
|
1,50 max |
| MATERIAL |
AVERAGE HARDNESS INDEX |
SPECIFIC WEIGHT |
| HASTELLOY B2 |
HRB 95 |
9,22 |
| HASTELLOY C276 |
HRB 90 |
8,88 |
| HASTELLOY D |
HRC 34 |
7,81 |
Diameters: from mm 3 to mm 150
Precision grades: ISO 3290 G100 - G200
|
|
 |
| 
|
|
|
|